TÝSESTER (PBT) / Teknik Özellikler
Û
Geri

Density

Ash Cont.

Hardness Shore

Tensile Strength

Elonga-
tion

Flex.Strength

Notched Impact Strength

Vicat Softening Temp.

HDT

Melting Rage

Flamma-bility

Test Methods

ISO1183

ISO 3451

 ISO  868

ISO 527

ISO527

ISO 178

ISO 180/A

ISO 306

ISO75 A/B

UL  94

UNIT

g / cm³

 %

 D

 MPa

 %

 MPa

 Kj / m²

 °C

 °C

 °C

UNR

PBTUNR1000

1. 31

80

57

40

83. 3

3. 1

216

57 / 154

220 – 225

HB

PBT UNR1010

1. 31

80

54

> 150

83. 3

4. 3

216

57 / 154

220 – 225

HB

Glass Fiber Reinf.

PBTGFR 15

1. 41

15

81

93. 1

4

147

7. 4

221

200 / 210

220 – 225

HB

PBTGFR 25

1. 45

25

82

119. 2

3. 3

179. 7

9. 8

221

207 / 213

220 – 225

HB

PBTGFR 30

1. 52

30

83

132. 3

3

196

11. 03

221

210 / 215

220 – 225

HB

Flame Retard.

PBT  FR

1. 44

80

61. 7

30

107. 8

3. 7

215

65 / 165

220 – 225

Vo

Copyright (C) Tisan A.Þ 2003