Processing Conditions

Injection Process Temperatures of Tisapet® PET

Predrying Tempereature

110-120 °C

Predrying Time

4-6 hours

Maximum Moisture

<0.015%

Melting Temperature

270-290 °C

Nozzle Temperature

270-290 °C

Pre-3 Region Temprature

270-290 °C

Mid-2 Region Temperature

270-290 °C

Aft-1 Region Temperature

270-280 °C

Mold Temperature

130-140 °C

Hold Pressure