Injection Process Temperatures of Hyperpol® SP |
|
|
Predrying Tempereature |
140-150 °C |
|
Predrying Time |
5-6 Hours |
|
Maximum Moisture |
- |
|
Melting Temperature |
320-340 °C |
|
Nozzle Temperature |
330-340 °C |
|
Pre-3 Region Temprature |
310-320 °C |
|
Mid-3 Region Temperature |
320-330 °C |
|
Aft-1 Region Temperature |
330-345 °C |
|
Mold Temperature |
140-170 °C |
|
Injection Process Temperatures of Hyperpol® AP |
|
|
Predrying Tempereature |
110-120 °C |
|
Predrying Time |
2-4 hours |
|
Maximum Moisture |
- |
|
Melting Temperature |
330-350 °C |
|
Nozzle Temperature |
330 °C |
|
Pre-3 Region Temprature |
330-340 °C |
|
Mid-3 Region Temperature |
330-340 °C |
|
Aft-1 Region Temperature |
330-340 °C |
|
Mold Temperature |
80-130 °C |